Monel 400 vs. PA 4/6
Monel 400 and PA 4/6 belong to fundamentally different material chemistries. Monel 400 is a metal, while PA 4/6 is a polymeric material. Therefore, their performance will be even more dissimilar than would be suggested by the difference in properties. There are 4 material properties with values for both materials. Properties with values for just one material (34, in this case) are not shown.
For each property being compared, the top bar is Monel 400 and the bottom bar is PA 4/6.
Metric UnitsUS Customary Units
Material Properties
Elastic (Young's, Tensile) Modulus, GPa | 160 | |
1.0 to 16 |
Elongation at Break, % | 20 to 40 | |
2.5 to 50 |
Melting Onset (Solidus), °C | 1300 | |
300 |
Tensile Strength: Ultimate (UTS), MPa | 540 to 780 | |
120 to 250 |