Monel 400 and PHB belong to fundamentally different material chemistries. Monel 400 is a metal, while PHB is a polymeric material. Therefore, their performance will be even more dissimilar than would be suggested by the difference in properties. There are 10 material properties with values for both materials. Properties with values for just one material (28, in this case) are not shown. Please note that the two materials have significantly dissimilar densities. This means that additional care is required when interpreting the data, because some material properties are based on units of mass, while others are based on units of area or volume.

For each property being compared, the top bar is Monel 400 and the bottom bar is PHB.

Metric UnitsUS Customary Units

Material Properties

Density, g/cm3 8.9
1.3
Elastic (Young's, Tensile) Modulus, GPa 160
1.3
Elongation at Break, % 20 to 40
7.5
Maximum Temperature: Mechanical, °C 1000
120
Melting Onset (Solidus), °C 1300
180
Stiffness to Weight: Axial, points 10
0.58
Stiffness to Weight: Bending, points 21
29
Strength to Weight: Axial, points 17 to 25
6.7
Strength to Weight: Bending, points 17 to 21
17
Tensile Strength: Ultimate (UTS), MPa 540 to 780
30