PA 4/6 vs. AWS E308Mo
PA 4/6 and AWS E308Mo belong to fundamentally different material chemistries. PA 4/6 is a polymeric material, while AWS E308Mo is a metal. Therefore, their performance will be even more dissimilar than would be suggested by the difference in properties. There are 4 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.
For each property being compared, the top bar is PA 4/6 and the bottom bar is AWS E308Mo.
Metric UnitsUS Customary Units
Material Properties
Elastic (Young's, Tensile) Modulus, GPa | 1.0 to 16 | |
200 |
Elongation at Break, % | 2.5 to 50 | |
40 |
Melting Onset (Solidus), °C | 300 | |
1400 |
Tensile Strength: Ultimate (UTS), MPa | 120 to 250 | |
620 |