MakeItFrom.com
Menu (ESC)

PA 4/6 vs. Austenitic Grey Cast Iron

PA 4/6 and austenitic grey cast iron belong to fundamentally different material chemistries. PA 4/6 is a polymeric material, while austenitic grey cast iron is a metal. Therefore, their performance will be even more dissimilar than would be suggested by the difference in properties. There are 3 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.

For each property being compared, the top bar is PA 4/6 and the bottom bar is austenitic grey cast iron.

Metric UnitsUS Customary Units

Material Properties

Elastic (Young's, Tensile) Modulus, GPa 1.0 to 16
180
Melting Onset (Solidus), °C 300
1290 to 1350
Tensile Strength: Ultimate (UTS), MPa 120 to 250
150 to 230