Density: 2.77 g/cm3 (173 lb/ft3)
Elastic (Young's, Tensile) Modulus: 73 GPa (11 x 106 psi)
Elongation at Break: 5 to 19 %
Melting Onset (Solidus): 502 °C (936 to 940 °F)
Specific Heat Capacity: 875 to 880 J/kg-K
Tensile Strength: Ultimate (UTS): 200 to 510 MPa (29 to 74 x 103 psi)
Tensile Strength: Yield (Proof): 81 to 470 MPa (12 to 68 x 103 psi)
Thermal Expansion: 23 µm/m-K
See Also
Aluminum Standards and Data, Aluminum Association Inc., 2013
ASTM B 209: Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate
ASTM B 210: Standard Specification for Aluminum and Aluminum-Alloy Drawn Seamless Tubes
ASTM B 211: Standard Specification for Aluminum and Aluminum-Alloy Bar, Rod, and Wire
ASTM B 221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes
ISO 6361: Wrought Aluminium and Aluminium Alloy Sheets, Strips and Plates