30% Carbon Fiber (30 CF) PSU

30 CF PSU is a grade of PSU. The graph bars on the material properties cards below compare 30 CF PSU to: sulfone plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Compressive (Crushing) Strength

95 MPa 14 x 103 psi

Elongation at Break

2.5 %

Flexural Modulus

14 GPa 2.0 x 106 psi

Flexural Strength

200 MPa 29 x 103 psi

Impact Strength: Notched Izod

59 J/m 1.1 ft-lb/in

Rockwell M Hardness

95

Tensile Strength: Ultimate (UTS)

130 MPa 19 x 103 psi

Thermal Properties

Heat Deflection Temperature At 1.82 MPa (264 psi)

200 °C 390 °F

Specific Heat Capacity

910 J/kg-K 0.22 BTU/lb-°F

Thermal Expansion

25 µm/m-K

Otherwise Unclassified Properties

Density

1.4 g/cm3 88 lb/ft3

Water Absorption At Saturation

0.4 %

Common Calculations

Strength to Weight: Axial

25 points

Strength to Weight: Bending

40 points

Followup Questions

Further Reading

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999