3003 (A93003) Aluminum
Material Properties
Density: 2.73 g/cm3 (170 lb/ft3)
Elastic (Young's, Tensile) Modulus: 69 GPa (10.0 x 106 psi)
Electrical Conductivity: 40 to 50 % IACS
Elongation at Break: 7 to 38 %
Fatigue Strength (Endurance Limit): 50 to 70 MPa (7.3 to 10 x 103 psi)
Fracture Toughness: 48 to 69 MPa-m1/2
Melting Onset (Solidus): 643 °C (1190 °F)
Shear Strength: 76 to 110 MPa (11 to 16 x 103 psi)
Specific Heat Capacity: 900 J/kg-K
Tensile Strength: Ultimate (UTS): 110 to 200 MPa (16 to 29 x 103 psi)
Tensile Strength: Yield (Proof): 42 to 190 MPa (6.1 to 28 x 103 psi)
Thermal Expansion: 23 µm/m-K
See Also
Aluminum Standards and Data, Aluminum Association Inc., 2013
ASTM B 209: Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate
ASTM B 210: Standard Specification for Aluminum and Aluminum-Alloy Drawn Seamless Tubes
ASTM B 211: Standard Specification for Aluminum and Aluminum-Alloy Bar, Rod, and Wire
ASTM B 221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes
ASTM B 483: Standard Specification for Aluminum and Aluminum-Alloy Drawn Tube and Pipe for General Purpose Applications
ASTM B 491: Standard Specification for Aluminum and Aluminum-Alloy Extruded Round Tubes for General-Purpose Applications
ASTM B 547: Standard Specification for Aluminum and Aluminum-Alloy Formed and Arc-Welded Round Tube
ISO 6361: Wrought Aluminium and Aluminium Alloy Sheets, Strips and Plates