6061 (A96061, AlMg1SiCu) Aluminum
Material Properties
Density: 2.70 g/cm3 (169 lb/ft3)
Elastic (Young's, Tensile) Modulus: 69 GPa (10.0 x 106 psi)
Elongation at Break: 6 to 22 %
Melting Onset (Solidus): 582 °C (1080 °F)
Specific Heat Capacity: 900 J/kg-K
Tensile Strength: Ultimate (UTS): 130 to 390 MPa (19 to 57 x 103 psi)
Tensile Strength: Yield (Proof): 64 to 350 MPa (9.3 to 51 x 103 psi)
Thermal Expansion: 24 µm/m-K
See Also
Aluminum Standards and Data, Aluminum Association Inc., 2013
ASTM B 209: Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate
ASTM B 210: Standard Specification for Aluminum and Aluminum-Alloy Drawn Seamless Tubes
ASTM B 211: Standard Specification for Aluminum and Aluminum-Alloy Bar, Rod, and Wire
ASTM B 221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes
ASTM B 308: Standard Specification for Aluminum-Alloy 6061-T6 Standard Structural Profiles
ASTM B 483: Standard Specification for Aluminum and Aluminum-Alloy Drawn Tube and Pipe for General Purpose Applications
ASTM B 547: Standard Specification for Aluminum and Aluminum-Alloy Formed and Arc-Welded Round Tube
ISO 6361: Wrought Aluminium and Aluminium Alloy Sheets, Strips and Plates