7075 (3.4365, L95, A97075) Aluminum
Material Properties
Base Metal Price: 10 % rel
Density: 2.80 g/cm3 (175 lb/ft3)
Elastic (Young's, Tensile) Modulus: 72 GPa (10 x 106 psi)
Electrical Conductivity: 33 to 40 % IACS
Elongation at Break: 13 to 14 %
Fatigue Strength (Endurance Limit): 160 MPa (23 x 103 psi)
Melting Onset (Solidus): 477 °C (891 °F)
Poisson's Ratio: 0.32
Shear Modulus: 27 GPa (3.9 106 psi)
Shear Strength: 152 to 331 MPa (22 to 48 x 103 psi)
Specific Heat Capacity: 960 J/kg-K
Tensile Strength: Ultimate (UTS): 240 to 570 MPa (35 to 83 x 103 psi)
Tensile Strength: Yield (Proof): 110 to 510 MPa (16 to 74 x 103 psi)
Thermal Conductivity: 130 to 160 W/m-K
Thermal Expansion: 23 to 23.2 µm/m-K
Alloy Composition
Aluminum (Al): 87.2 to 91.4 %
Zinc (Zn): 5.1 to 6.1 %
Magnesium (Mg): 2.1 to 2.9 %
Copper (Cu): 1.2 to 2.0 %
Iron (Fe): 0 to 0.5 %
Silicon (Si): 0 to 0.4 %
Manganese (Mn): 0 to 0.30 %
Chromium (Cr): 0.18 to 0.28 %
Zirconium (Zr): 0 to 0.25 %
Titanium (Ti): 0 to 0.2 %
Residuals: 0 to 0.15 %
See Also
Aluminum Standards and Data, Aluminum Association Inc., 2013
ASTM B 209: Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate
ASTM B 210: Standard Specification for Aluminum and Aluminum-Alloy Drawn Seamless Tubes
ASTM B 211: Standard Specification for Aluminum and Aluminum-Alloy Bar, Rod, and Wire
ASTM B 221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes