ASTM CA40 (SCS2A, J91153) Cast Stainless Steel
Material Properties
Density: 7.6 g/cm3 (470 lb/ft3)
Elastic (Young's, Tensile) Modulus: 200 GPa (29 x 106 psi)
Electrical Conductivity: 3 % IACS
Elongation at Break: 10 %
Melting Onset (Solidus): 1500 °C (2730 °F)
Specific Heat Capacity: 460 J/kg-K
Tensile Strength: Ultimate (UTS): 1030 MPa (150 x 103 psi)
Tensile Strength: Yield (Proof): 860 MPa (125 x 103 psi)
Thermal Conductivity: 25 W/m-K
Thermal Expansion: 10 µm/m-K
See Also
Corrosion Resistance of Stainless Steels, C. P. Dillon, 1995