ASTM D787 Grade 11 Ethyl Cellulose

Grade 11 EC is a grade of Ethyl Cellulose. It has the lowest strength compared to the other variants of Ethyl Cellulose. The graph bars on the material properties cards below compare grade 11 EC to: cellulosic plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Impact Strength: Notched Izod

220 J/m 4.2 ft-lb/in

Rockwell R Hardness

56

Tensile Strength: Ultimate (UTS)

18 MPa 2.6 x 103 psi

Other Material Properties

Density

1.1 g/cm3 69 lb/ft3

Heat Deflection Temperature At 1.82 MPa (264 psi)

56 °C 130 °F

Water Absorption After 24 Hours

1.3 %

Common Calculations

Strength to Weight: Axial

4.6 points

Strength to Weight: Bending

14 points

Followup Questions

Further Reading

ASTM D787: Standard Specification for Ethyl Cellulose Molding and Extrusion Compounds