Conditioned 30% Glass Fiber (30 GF) PA 6

Conditioned 30 GF PA 6 is a grade of PA 6. The graph bars on the material properties cards below compare conditioned 30 GF PA 6 to: polyamide plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

6.0 GPa 0.87 x 106 psi

Elongation at Break

5.0 %

Flexural Modulus

2.4 GPa 0.35 x 106 psi

Flexural Strength

110 MPa 16 x 103 psi

Tensile Strength: Ultimate (UTS)

110 MPa 16 x 103 psi

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz

20

Dielectric Constant (Relative Permittivity) At 1 MHz

5.0

Dielectric Strength (Breakdown Potential)

25 kV/mm 1.0 V/mil

Electrical Resistivity Order of Magnitude

11 10x Ω-m

Other Material Properties

Glass Transition Temperature

40 °C 100 °F

Limiting Oxygen Index (LOI)

24 %

Maximum Temperature: Autoignition

430 °C 810 °F

Maximum Temperature: Decomposition

430 °C 800 °F

Melting Onset (Solidus)

230 °C 450 °F

Followup Questions

Further Reading

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999