Conditioned Unfilled PA 4/6

Conditioned unfilled PA 4/6 is a grade of PA 4/6. It has the highest ductility compared to the other variants of PA 4/6. The graph bars on the material properties cards below compare conditioned unfilled PA 4/6 to: polyamide plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

1.0 GPa 0.15 x 106 psi

Elongation at Break

50 %

Flexural Modulus

0.9 GPa 0.13 x 106 psi

Flexural Strength

50 MPa 7.3 x 103 psi

Tensile Strength: Yield (Proof)

55 MPa 8.0 x 103 psi

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz

22

Dielectric Constant (Relative Permittivity) At 1 MHz

4.5

Dielectric Strength (Breakdown Potential)

15 kV/mm 0.59 V/mil

Electrical Resistivity Order of Magnitude

7.0 10x Ω-m

Other Material Properties

Melting Onset (Solidus)

300 °C 560 °F

Common Calculations

Resilience: Unit (Modulus of Resilience)

1510 kJ/m3

Followup Questions

Further Reading

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999