Hot Rolled SAE-AISI 1040 Carbon Steel
Material Properties
Density: 7.8 g/cm3 (490 lb/ft3)
Elongation at Break: 22 %
Tensile Strength: Ultimate (UTS): 550 MPa (80 x 103 psi)
Tensile Strength: Yield (Proof): 320 MPa (46 x 103 psi)