ASTM A217 Cast Steel vs. EN 2.4878 Nickel

ASTM A217 cast steel belongs to the iron alloys classification, while EN 2.4878 nickel belongs to the nickel alloys. There are 27 material properties with values for both materials. Properties with values for just one material (6, in this case) are not shown.

For each property being compared, the top bar is ASTM A217 cast steel and the bottom bar is EN 2.4878 nickel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
200
Elongation at Break, % 21 to 27
13 to 17
Fatigue Strength, MPa 200 to 320
400 to 410
Poisson's Ratio 0.28 to 0.29
0.29
Shear Modulus, GPa 73 to 75
78
Tensile Strength: Ultimate (UTS), MPa 540 to 710
1210 to 1250
Tensile Strength: Yield (Proof), MPa 270 to 460
740 to 780

Thermal Properties

Latent Heat of Fusion, J/g 250 to 270
330
Maximum Temperature: Mechanical, °C 410 to 600
1030
Melting Completion (Liquidus), °C 1450 to 1460
1370
Melting Onset (Solidus), °C 1410 to 1420
1320
Specific Heat Capacity, J/kg-K 470
460
Thermal Conductivity, W/m-K 26 to 50
11
Thermal Expansion, µm/m-K 13
12

Otherwise Unclassified Properties

Base Metal Price, % relative 2.4 to 7.0
80
Density, g/cm3 7.8
8.3
Embodied Carbon, kg CO2/kg material 1.5 to 2.1
10
Embodied Energy, MJ/kg 20 to 28
150
Embodied Water, L/kg 47 to 87
370

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 110 to 130
150 to 180
Resilience: Unit (Modulus of Resilience), kJ/m3 190 to 570
1370 to 1540
Stiffness to Weight: Axial, points 13 to 14
13
Stiffness to Weight: Bending, points 24 to 25
24
Strength to Weight: Axial, points 19 to 25
41 to 42
Strength to Weight: Bending, points 19 to 23
31
Thermal Diffusivity, mm2/s 6.9 to 14
2.8
Thermal Shock Resistance, points 16 to 20
37 to 39