ASTM A228 Music Wire vs. ASTM A209 Steel

Both ASTM A228 music wire and ASTM A209 steel are iron alloys. There are 30 material properties with values for both materials. Properties with values for just one material (2, in this case) are not shown.

For each property being compared, the top bar is ASTM A228 music wire and the bottom bar is ASTM A209 steel.

Metric UnitsUS Customary Units

Mechanical Properties

Brinell Hardness 710
140 to 150
Elastic (Young's, Tensile) Modulus, GPa 190
190
Elongation at Break, % 12
34
Fatigue Strength, MPa 1280
180 to 200
Poisson's Ratio 0.29
0.29
Shear Modulus, GPa 72
73
Shear Strength, MPa 1470
280 to 310
Tensile Strength: Ultimate (UTS), MPa 2450
420 to 460
Tensile Strength: Yield (Proof), MPa 2050
220 to 250

Thermal Properties

Latent Heat of Fusion, J/g 250
250
Maximum Temperature: Mechanical, °C 400
410
Melting Completion (Liquidus), °C 1450
1470
Melting Onset (Solidus), °C 1410
1420 to 1430
Specific Heat Capacity, J/kg-K 470
470
Thermal Conductivity, W/m-K 49
50
Thermal Expansion, µm/m-K 12
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.1
7.1
Electrical Conductivity: Equal Weight (Specific), % IACS 8.2
8.1 to 8.2

Otherwise Unclassified Properties

Base Metal Price, % relative 1.8
2.4
Density, g/cm3 7.8
7.9
Embodied Carbon, kg CO2/kg material 1.4
1.5
Embodied Energy, MJ/kg 19
20
Embodied Water, L/kg 45
47

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 280
120 to 130
Stiffness to Weight: Axial, points 13
13
Stiffness to Weight: Bending, points 24
24
Strength to Weight: Axial, points 87
15 to 16
Strength to Weight: Bending, points 52
16 to 17
Thermal Diffusivity, mm2/s 13
13
Thermal Shock Resistance, points 79
12 to 14