Elastic (Young's, Tensile) Modulus, GPa 190
140
Elongation at Break, % 25 to 27
20
Poisson's Ratio 0.29
0.33
Shear Modulus, GPa 73
53
Tensile Strength: Ultimate (UTS), MPa 460 to 550
490
Tensile Strength: Yield (Proof), MPa 230 to 310
290

Thermal Properties

Latent Heat of Fusion, J/g 250
240
Maximum Temperature: Mechanical, °C 400
260
Melting Completion (Liquidus), °C 1460
1180
Melting Onset (Solidus), °C 1420
1120
Specific Heat Capacity, J/kg-K 470
410
Thermal Conductivity, W/m-K 52
30
Thermal Expansion, µm/m-K 12
15

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.0 to 7.1
5.5
Electrical Conductivity: Equal Weight (Specific), % IACS 8.1
5.6

Otherwise Unclassified Properties

Base Metal Price, % relative 1.8
41
Density, g/cm3 7.8
8.9
Embodied Carbon, kg CO2/kg material 1.4
5.2
Embodied Energy, MJ/kg 18
76
Embodied Water, L/kg 45 to 46
290

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 96 to 120
85
Resilience: Unit (Modulus of Resilience), kJ/m3 140 to 260
290
Stiffness to Weight: Axial, points 13
8.8
Stiffness to Weight: Bending, points 24
20
Strength to Weight: Axial, points 16 to 20
15
Strength to Weight: Bending, points 17 to 19
16
Thermal Diffusivity, mm2/s 14
8.2
Thermal Shock Resistance, points 15 to 18
16