ASTM A387 grade 12 class 1 belongs to the iron alloys classification, while annealed 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.

For each property being compared, the top bar is ASTM A387 grade 12 class 1 and the bottom bar is annealed 92-silver 8-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 7.2
80
Elongation at Break, % 25
32
Resilience: Ultimate (Unit Rupture Work), MJ/m3 98
62
Shear Strength, MPa 300
150
Tensile Strength: Ultimate (UTS), MPa 470
230
Tensile Strength: Yield (Proof), MPa 260
120