AWS ERTi-2 belongs to the titanium alloys classification, while ASTM A209 steel belongs to the iron alloys. There are 29 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is AWS ERTi-2 and the bottom bar is ASTM A209 steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 110
190
Elongation at Break, % 20
34
Fatigue Strength, MPa 190
180 to 200
Poisson's Ratio 0.32
0.29
Shear Modulus, GPa 40
73
Tensile Strength: Ultimate (UTS), MPa 340
420 to 460
Tensile Strength: Yield (Proof), MPa 280
220 to 250

Thermal Properties

Latent Heat of Fusion, J/g 420
250
Maximum Temperature: Mechanical, °C 320
410
Melting Completion (Liquidus), °C 1670
1470
Melting Onset (Solidus), °C 1620
1420 to 1430
Specific Heat Capacity, J/kg-K 540
470
Thermal Conductivity, W/m-K 21
50
Thermal Expansion, µm/m-K 8.7
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 3.6
7.1
Electrical Conductivity: Equal Weight (Specific), % IACS 7.1
8.1 to 8.2

Otherwise Unclassified Properties

Base Metal Price, % relative 37
2.4
Density, g/cm3 4.5
7.9
Embodied Carbon, kg CO2/kg material 31
1.5
Embodied Energy, MJ/kg 510
20
Embodied Water, L/kg 110
47

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 64
120 to 130
Resilience: Unit (Modulus of Resilience), kJ/m3 360
130 to 170
Stiffness to Weight: Axial, points 13
13
Stiffness to Weight: Bending, points 35
24
Strength to Weight: Axial, points 21
15 to 16
Strength to Weight: Bending, points 24
16 to 17
Thermal Diffusivity, mm2/s 8.7
13
Thermal Shock Resistance, points 27
12 to 14