Material Properties
Density, g/cm3 | 9.9 | |
17 |
Elongation at Break, % | 15 | |
28 |
Strength to Weight: Axial, points | 8.8 | |
3.6 |
Strength to Weight: Bending, points | 10 | |
4.8 |
Tensile Strength: Ultimate (UTS), MPa | 310 | |
210 |