Electrical Conductivity: Equal Volume, % IACS 86
3.7
Elongation at Break, % 37
35
Resilience: Ultimate (Unit Rupture Work), MJ/m3 70
160
Shear Strength, MPa 150
350
Tensile Strength: Ultimate (UTS), MPa 230
520
Tensile Strength: Yield (Proof), MPa 110
350