Annealed 90-silver 10-tin-oxide vs. Annealed 92-silver 8-tin-oxide
Both annealed 90-silver 10-tin-oxide and annealed 92-silver 8-tin-oxide are otherwise unclassified metals. Both are furnished in the annealed condition.
For each property being compared, the top bar is annealed 90-silver 10-tin-oxide and the bottom bar is annealed 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
| Electrical Conductivity: Equal Volume, % IACS | 82 | |
| 80 | 
| Elongation at Break, % | 35 | |
| 32 | 
| Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 68 | |
| 62 | 
| Shear Strength, MPa | 160 | |
| 150 | 
| Tensile Strength: Ultimate (UTS), MPa | 230 | |
| 230 | 
| Tensile Strength: Yield (Proof), MPa | 120 | |
| 120 |