Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 110
190
Elongation at Break, % 15
25 to 27
Poisson's Ratio 0.34
0.29
Shear Modulus, GPa 40
72
Tensile Strength: Ultimate (UTS), MPa 230
500 to 570
Tensile Strength: Yield (Proof), MPa 110
230 to 310

Thermal Properties

Latent Heat of Fusion, J/g 190
250
Maximum Temperature: Mechanical, °C 160
400
Melting Completion (Liquidus), °C 980
1450 to 1460
Melting Onset (Solidus), °C 910
1410
Specific Heat Capacity, J/kg-K 370
470
Thermal Conductivity, W/m-K 72
49 to 52
Thermal Expansion, µm/m-K 19
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 16
7.1 to 7.2
Electrical Conductivity: Equal Weight (Specific), % IACS 16
8.2 to 8.3

Otherwise Unclassified Properties

Base Metal Price, % relative 30
1.8
Density, g/cm3 8.8
7.8
Embodied Carbon, kg CO2/kg material 2.9
1.4
Embodied Energy, MJ/kg 47
18
Embodied Water, L/kg 340
45

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 28
110 to 120
Resilience: Unit (Modulus of Resilience), kJ/m3 54
140 to 250
Stiffness to Weight: Axial, points 6.8
13
Stiffness to Weight: Bending, points 18
24
Strength to Weight: Axial, points 7.3
18 to 20
Strength to Weight: Bending, points 9.5
18 to 20
Thermal Diffusivity, mm2/s 22
13 to 14
Thermal Shock Resistance, points 8.2
16 to 18