Full-hard 85-silver 15-nickel vs. Full-hard K93600

Full-hard 85-silver 15-nickel belongs to the otherwise unclassified metals classification, while full-hard K93600 belongs to the iron alloys. There are 13 material properties with values for both materials. Properties with values for just one material (11, in this case) are not shown.

For each property being compared, the top bar is full-hard 85-silver 15-nickel and the bottom bar is full-hard K93600.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 88
140
Tensile Strength: Ultimate (UTS), MPa 450
810

Thermal Properties

Melting Onset (Solidus), °C 960
1430
Specific Heat Capacity, J/kg-K 270
520
Thermal Expansion, µm/m-K 18
7.3

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 86
2.2
Electrical Conductivity: Equal Weight (Specific), % IACS 75
2.4

Otherwise Unclassified Properties

Density, g/cm3 10
8.1

Common Calculations

Stiffness to Weight: Axial, points 4.8
9.4
Stiffness to Weight: Bending, points 14
21
Strength to Weight: Axial, points 12
28
Strength to Weight: Bending, points 13
24
Thermal Shock Resistance, points 20
57