MakeItFrom.com
Menu (ESC)

Half-hard ASTM F15 vs. Half-hard K93600

Both half-hard ASTM F15 and half-hard K93600 are iron alloys. Both are furnished in the half-hard temper. There are 16 material properties with values for both materials. Properties with values for just one material (14, in this case) are not shown.

For each property being compared, the top bar is half-hard ASTM F15 and the bottom bar is half-hard K93600.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
140
Tensile Strength: Ultimate (UTS), MPa 680
650

Thermal Properties

Curie Temperature, °C 430
250
Melting Onset (Solidus), °C 1450
1430
Specific Heat Capacity, J/kg-K 460
520
Thermal Conductivity, W/m-K 17
13
Thermal Expansion, µm/m-K 6.0
7.3

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 3.7
2.2
Electrical Conductivity: Equal Weight (Specific), % IACS 4.0
2.4

Otherwise Unclassified Properties

Density, g/cm3 8.3
8.1

Common Calculations

Stiffness to Weight: Axial, points 13
9.4
Stiffness to Weight: Bending, points 23
21
Strength to Weight: Axial, points 23
22
Strength to Weight: Bending, points 21
21
Thermal Diffusivity, mm2/s 4.5
3.1
Thermal Shock Resistance, points 42
47