Both half-hard K93600 and half-hard K93603 alloy are iron alloys. Both are furnished in the half-hard temper. There are 11 material properties with values for both materials. Properties with values for just one material (19, in this case) are not shown.

For each property being compared, the top bar is half-hard K93600 and the bottom bar is half-hard K93603 alloy.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 140
190
Tensile Strength: Ultimate (UTS), MPa 650
680

Thermal Properties

Melting Onset (Solidus), °C 1430
1380
Specific Heat Capacity, J/kg-K 520
460
Thermal Expansion, µm/m-K 7.3
12

Otherwise Unclassified Properties

Density, g/cm3 8.1
8.2

Common Calculations

Stiffness to Weight: Axial, points 9.4
13
Stiffness to Weight: Bending, points 21
23
Strength to Weight: Axial, points 22
23
Strength to Weight: Bending, points 21
21
Thermal Shock Resistance, points 47
21