Brinell Hardness 14
240 to 250
Elastic (Young's, Tensile) Modulus, GPa 38
190
Elongation at Break, % 48
18 to 21
Poisson's Ratio 0.39
0.29
Shear Modulus, GPa 14
73
Tensile Strength: Ultimate (UTS), MPa 31
790 to 830
Tensile Strength: Yield (Proof), MPa 27
690 to 770

Thermal Properties

Latent Heat of Fusion, J/g 46
250 to 260
Melting Completion (Liquidus), °C 180
1460
Melting Onset (Solidus), °C 180
1420
Specific Heat Capacity, J/kg-K 190
470
Thermal Conductivity, W/m-K 51
37 to 51
Thermal Expansion, µm/m-K 25
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 12
7.2 to 7.6
Electrical Conductivity: Equal Weight (Specific), % IACS 12
8.3 to 8.8

Otherwise Unclassified Properties

Density, g/cm3 8.8
7.8 to 7.9
Embodied Carbon, kg CO2/kg material 11
1.6 to 1.8
Embodied Energy, MJ/kg 180
21 to 25
Embodied Water, L/kg 930
48 to 57

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 14
140 to 170
Resilience: Unit (Modulus of Resilience), kJ/m3 9.9
1280 to 1590
Stiffness to Weight: Axial, points 2.4
13
Stiffness to Weight: Bending, points 13
24
Strength to Weight: Axial, points 1.0
28 to 29
Strength to Weight: Bending, points 2.5
24 to 25
Thermal Diffusivity, mm2/s 31
10 to 14
Thermal Shock Resistance, points 2.4
23 to 24