Material Properties

Density, g/cm3 1.3
1.2
Elongation at Break, % 2.0
400
Glass Transition Temperature, °C 170
0
Limiting Oxygen Index (LOI), % 27
25
Maximum Temperature: Mechanical, °C 150
120
Strength to Weight: Axial, points 10
2.1
Strength to Weight: Bending, points 23
8.0
Tensile Strength: Ultimate (UTS), MPa 48
9.0