Soda-lime Glass vs. Tempered Soda-lime Glass
Tempered soda-lime glass is a variant of soda-lime glass. The properties of the parent material encompass the values of all of its variants.
For each property being compared, the top bar is soda-lime glass and the bottom bar is tempered soda-lime glass.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 70 to 71 | |
70 |
Knoop Hardness | 570 | |
570 |
Poisson's Ratio | 0.23 | |
0.23 |
Shear Modulus, GPa | 29 | |
29 |
Tensile Strength: Ultimate (UTS), MPa | 41 to 180 | |
180 |
Thermal Properties
Maximum Temperature: Mechanical, °C | 300 | |
300 |
Specific Heat Capacity, J/kg-K | 720 to 800 | |
720 |
Thermal Conductivity, W/m-K | 1.0 to 1.1 | |
1.1 |
Thermal Expansion, µm/m-K | 8.8 to 9.0 | |
9.0 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 MHz | 7.3 to 7.4 | |
7.3 |
Dielectric Strength (Breakdown Potential), kV/mm | 13 | |
13 |
Otherwise Unclassified Properties
Density, g/cm3 | 2.4 | |
2.4 |
Light Transmission Range, µm | 0.35 to 2.5 | |
0.35 to 2.5 |
Refractive Index | 1.5 | |
1.5 |
Common Calculations
Stiffness to Weight: Axial, points | 16 | |
16 |
Stiffness to Weight: Bending, points | 56 | |
56 |
Strength to Weight: Axial, points | 4.6 to 20 | |
20 |
Strength to Weight: Bending, points | 11 to 28 | |
28 |
Thermal Diffusivity, mm2/s | 0.51 to 0.6 | |
0.6 |
Thermal Shock Resistance, points | 4.7 to 20 | |
20 |