C96600 copper belongs to the copper alloys classification, while ASTM A283 carbon steel belongs to the iron alloys. There are 28 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is C96600 copper and the bottom bar is ASTM A283 carbon steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 140
190
Elongation at Break, % 7.0
26 to 34
Poisson's Ratio 0.33
0.29
Shear Modulus, GPa 52
73
Tensile Strength: Ultimate (UTS), MPa 760
360 to 480
Tensile Strength: Yield (Proof), MPa 480
180 to 260

Thermal Properties

Latent Heat of Fusion, J/g 240
250
Maximum Temperature: Mechanical, °C 280
400
Melting Completion (Liquidus), °C 1180
1460
Melting Onset (Solidus), °C 1100
1420
Specific Heat Capacity, J/kg-K 400
470
Thermal Conductivity, W/m-K 30
51 to 53
Thermal Expansion, µm/m-K 15
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 4.0
7.1
Electrical Conductivity: Equal Weight (Specific), % IACS 4.1
8.1

Otherwise Unclassified Properties

Base Metal Price, % relative 65
1.8
Density, g/cm3 8.9
7.8 to 7.9
Embodied Carbon, kg CO2/kg material 7.0
1.4
Embodied Energy, MJ/kg 100
18
Embodied Water, L/kg 280
46

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 47
100 to 110
Resilience: Unit (Modulus of Resilience), kJ/m3 830
91 to 180
Stiffness to Weight: Axial, points 8.7
13
Stiffness to Weight: Bending, points 20
24
Strength to Weight: Axial, points 24
13 to 17
Strength to Weight: Bending, points 21
14 to 17
Thermal Diffusivity, mm2/s 8.4
14
Thermal Shock Resistance, points 25
11 to 15