Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 140
140
Poisson's Ratio 0.34
0.37
Shear Modulus, GPa 54
50
Tensile Strength: Ultimate (UTS), MPa 500 to 710
210

Thermal Properties

Melting Onset (Solidus), °C 1440
1140
Specific Heat Capacity, J/kg-K 500
280
Thermal Expansion, µm/m-K 5.0
12

Otherwise Unclassified Properties

Density, g/cm3 8.2
13

Common Calculations

Stiffness to Weight: Axial, points 9.8
5.8
Stiffness to Weight: Bending, points 21
13
Strength to Weight: Axial, points 17 to 24
4.5
Strength to Weight: Bending, points 17 to 22
6.0
Thermal Shock Resistance, points 49 to 70
9.0