MakeItFrom.com
Menu (ESC)

Work Hardened 88-silver 12-tin-oxide vs. Work Hardened ASTM B522 Class I

Both work hardened 88-silver 12-tin-oxide and work hardened ASTM B522 class I are otherwise unclassified metals. Both are furnished in the cold worked (strain hardened) condition. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.

For each property being compared, the top bar is work hardened 88-silver 12-tin-oxide and the bottom bar is work hardened ASTM B522 class I.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 84
11
Elongation at Break, % 9.0
1.1
Resilience: Ultimate (Unit Rupture Work), MJ/m3 24
4.5
Shear Strength, MPa 160
280
Tensile Strength: Ultimate (UTS), MPa 280
490
Tensile Strength: Yield (Proof), MPa 260
210