Both work hardened 90-silver 10-tin-oxide and work hardened ASTM B522 class II are otherwise unclassified metals. Both are furnished in the cold worked (strain hardened) condition. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.

For each property being compared, the top bar is work hardened 90-silver 10-tin-oxide and the bottom bar is work hardened ASTM B522 class II.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 77
11
Elongation at Break, % 7.0
1.1
Resilience: Ultimate (Unit Rupture Work), MJ/m3 20
4.4
Shear Strength, MPa 170
280
Tensile Strength: Ultimate (UTS), MPa 300
490
Tensile Strength: Yield (Proof), MPa 280
210