3/4-Hard (H03) C19010 Copper
H03 C19010 copper is C19010 copper in the H03 (3/4 hard) temper. The graph bars on the material properties cards below compare H03 C19010 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elastic (Young's, Tensile) Modulus
120 GPa 17 x 106 psi
Elongation at Break
6.1 %
Poisson's Ratio
0.34
Shear Modulus
43 GPa 6.3 x 106 psi
Shear Strength
270 MPa 40 x 103 psi
Tensile Strength: Ultimate (UTS)
470 MPa 68 x 103 psi
Tensile Strength: Yield (Proof)
450 MPa 65 x 103 psi
Thermal Properties
Latent Heat of Fusion
210 J/g
Maximum Temperature: Mechanical
200 °C 400 °F
Melting Completion (Liquidus)
1060 °C 1940 °F
Melting Onset (Solidus)
1010 °C 1850 °F
Specific Heat Capacity
390 J/kg-K 0.093 BTU/lb-°F
Thermal Conductivity
260 W/m-K 150 BTU/h-ft-°F
Thermal Expansion
17 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
50 % IACS
Electrical Conductivity: Equal Weight (Specific)
50 % IACS
Otherwise Unclassified Properties
Base Metal Price
31 % relative
Density
8.9 g/cm3 560 lb/ft3
Embodied Carbon
2.7 kg CO2/kg material
Embodied Energy
42 MJ/kg 18 x 103 BTU/lb
Embodied Water
310 L/kg 37 gal/lb
Common Calculations
Resilience: Ultimate (Unit Rupture Work)
28 MJ/m3
Resilience: Unit (Modulus of Resilience)
850 kJ/m3
Stiffness to Weight: Axial
7.3 points
Stiffness to Weight: Bending
18 points
Strength to Weight: Axial
15 points
Strength to Weight: Bending
15 points
Thermal Diffusivity
75 mm2/s
Thermal Shock Resistance
17 points
Alloy Composition
| Cu | 97.3 to 99.04 | |
| Ni | 0.8 to 1.8 | |
| Si | 0.15 to 0.35 | |
| P | 0.010 to 0.050 | |
| res. | 0 to 0.5 |
All values are % weight. Ranges represent what is permitted under applicable standards.
Followup Questions
Further Reading
ASTM B422: Standard Specification for Copper-Aluminum-Silicon-Cobalt Alloy, Copper-Nickel-Silicon-Magnesium Alloy, Copper-Nickel-Silicon Alloy, Copper-Nickel-Aluminum-Magnesium Alloy, and Copper- Nickel-Tin Alloy Sheet and Strip
Copper: Its Trade, Manufacture, Use, and Environmental Status, Gunter Joseph, 2001