30 GF PC is a grade of PC. The graph bars on the material properties cards below compare 30 GF PC to: otherwise unclassified thermoplastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

4.0 %

Flexural Modulus

8.2 GPa 1.2 x 106 psi

Flexural Strength

160 MPa 22 x 103 psi

Impact Strength: Notched Izod

140 J/m 2.6 ft-lb/in

Rockwell M Hardness

92

Tensile Strength: Ultimate (UTS)

130 MPa 19 x 103 psi

Thermal Properties

Glass Transition Temperature

150 °C 300 °F

Heat Deflection Temperature At 1.82 MPa (264 psi)

140 °C 290 °F

Specific Heat Capacity

1040 J/kg-K 0.25 BTU/lb-°F

Thermal Expansion

10 µm/m-K

Otherwise Unclassified Properties

Density

1.4 g/cm3 88 lb/ft3

Water Absorption At Saturation

0.18 %

Common Calculations

Strength to Weight: Axial

26 points

Strength to Weight: Bending

41 points

Followup Questions

Further Reading

ASTM D883: Standard Terminology Relating to Plastics

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999