MakeItFrom.com
Menu (ESC)

30% Glass Fiber (30 GF) POM-C

30 GF POM-C is a grade of POM-C. The graph bars on the material properties cards below compare 30 GF POM-C to: polyoxymethylene plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elastic (Young's, Tensile) Modulus

9.7 GPa 1.4 x 106 psi

Elongation at Break

3.0 %

Flexural Modulus

9.0 GPa 1.3 x 106 psi

Flexural Strength

170 MPa 25 x 103 psi

Impact Strength: Notched Izod

68 J/m 1.3 ft-lb/in

Tensile Strength: Ultimate (UTS)

110 MPa 16 x 103 psi

Other Material Properties

Density

1.6 g/cm3 100 lb/ft3

Limiting Oxygen Index (LOI)

15 %

Specific Heat Capacity

1130 J/kg-K 0.27 BTU/lb-°F

Water Absorption At Saturation

1.4 %

Common Calculations

Stiffness to Weight: Axial

3.3 points

Stiffness to Weight: Bending

44 points

Strength to Weight: Axial

19 points

Strength to Weight: Bending

32 points

Followup Questions

Further Reading

Reinforced Plastics Durability, Geoffrey Pritchard (editor), 1999

SPI Plastics Engineering Handbook of the Society of the Plastics Industry, Inc., 5th ed., Michael L. Berins (editor), 2000

Modern Plastics Handbook, Charles A. Harper (editor), 1999

Plastics Materials, 7th ed., J. A. Brydson, 1999