6162-T5 Aluminum
6162-T5 aluminum is 6162 aluminum in the T5 temper. To achieve this temper, the metal is artificially aged until it meets standard mechanical property requirements. The graph bars on the material properties cards below compare 6162-T5 aluminum to: 6000-series alloys (top), all aluminum alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elastic (Young's, Tensile) Modulus
68 GPa 9.9 x 106 psi
Elongation at Break
6.8 %
Fatigue Strength
120 MPa 18 x 103 psi
Poisson's Ratio
0.33
Shear Modulus
26 GPa 3.7 x 106 psi
Shear Strength
170 MPa 25 x 103 psi
Tensile Strength: Ultimate (UTS)
290 MPa 42 x 103 psi
Tensile Strength: Yield (Proof)
260 MPa 38 x 103 psi
Thermal Properties
Latent Heat of Fusion
400 J/g
Maximum Temperature: Mechanical
160 °C 320 °F
Melting Completion (Liquidus)
640 °C 1190 °F
Melting Onset (Solidus)
620 °C 1140 °F
Specific Heat Capacity
900 J/kg-K 0.22 BTU/lb-°F
Thermal Conductivity
190 W/m-K 110 BTU/h-ft-°F
Thermal Expansion
23 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
50 % IACS
Electrical Conductivity: Equal Weight (Specific)
170 % IACS
Otherwise Unclassified Properties
Base Metal Price
9.5 % relative
Density
2.7 g/cm3 170 lb/ft3
Embodied Carbon
8.3 kg CO2/kg material
Embodied Energy
150 MJ/kg 66 x 103 BTU/lb
Embodied Water
1180 L/kg 140 gal/lb
Common Calculations
Resilience: Ultimate (Unit Rupture Work)
19 MJ/m3
Resilience: Unit (Modulus of Resilience)
510 kJ/m3
Stiffness to Weight: Axial
14 points
Stiffness to Weight: Bending
50 points
Strength to Weight: Axial
30 points
Strength to Weight: Bending
36 points
Thermal Diffusivity
79 mm2/s
Thermal Shock Resistance
13 points
Alloy Composition
| Al | 96.7 to 98.9 | |
| Mg | 0.7 to 1.1 | |
| Si | 0.4 to 0.8 | |
| Fe | 0 to 0.5 | |
| Zn | 0 to 0.25 | |
| Cu | 0 to 0.2 | |
| Mn | 0 to 0.1 | |
| Cr | 0 to 0.1 | |
| Ti | 0 to 0.1 | |
| res. | 0 to 0.15 |
All values are % weight. Ranges represent what is permitted under applicable standards.
Followup Questions
Further Reading
ASTM B221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes
Aluminum Standards and Data, Aluminum Association Inc., 2013
ASM Specialty Handbook: Aluminum and Aluminum Alloys, J. R. Davis (editor), 1993