MakeItFrom.com
Menu (ESC)

ASTM D787 Grade 1 Ethyl Cellulose

Grade 1 EC is a grade of Ethyl Cellulose. It has the highest strength compared to the other variants of Ethyl Cellulose. The graph bars on the material properties cards below compare grade 1 EC to: cellulosic plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Impact Strength: Notched Izod

66 J/m 1.2 ft-lb/in

Rockwell R Hardness

120

Tensile Strength: Ultimate (UTS)

51 MPa 7.4 x 103 psi

Thermal Properties

Heat Deflection Temperature At 1.82 MPa (264 psi)

93 °C 200 °F

Heat Deflection Temperature At 455 kPa (66 psi)

110 °C 220 °F

Otherwise Unclassified Properties

Density

1.1 g/cm3 71 lb/ft3

Water Absorption After 24 Hours

1.5 %

Common Calculations

Strength to Weight: Axial

13 points

Strength to Weight: Bending

27 points

Followup Questions

Further Reading

ASTM D787: Standard Specification for Ethyl Cellulose Molding and Extrusion Compounds