ASTM D787 Grade 2 Ethyl Cellulose

Grade 2 EC is a grade of Ethyl Cellulose. It has the second highest strength compared to the other variants of Ethyl Cellulose. The graph bars on the material properties cards below compare grade 2 EC to: cellulosic plastics (top), all thermoplastics (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Impact Strength: Notched Izod

67 J/m 1.3 ft-lb/in

Rockwell R Hardness

130

Tensile Strength: Ultimate (UTS)

46 MPa 6.7 x 103 psi

Thermal Properties

Heat Deflection Temperature At 1.82 MPa (264 psi)

86 °C 190 °F

Heat Deflection Temperature At 455 kPa (66 psi)

100 °C 210 °F

Otherwise Unclassified Properties

Density

1.1 g/cm3 71 lb/ft3

Water Absorption After 24 Hours

1.3 %

Common Calculations

Strength to Weight: Axial

11 points

Strength to Weight: Bending

25 points

Followup Questions

Further Reading

ASTM D787: Standard Specification for Ethyl Cellulose Molding and Extrusion Compounds