Annealed 86.5-silver 13.5-cadmium-oxide is 86.5-silver 13.5-cadmium-oxide in the annealed condition. It has the lowest strength compared to the other variants of 86.5-silver 13.5-cadmium-oxide.

The graph bars on the material properties cards below compare annealed 86.5-silver 13.5-cadmium-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

16 %

Shear Strength

170 MPa 25 x 103 psi

Tensile Strength: Ultimate (UTS)

280 MPa 40 x 103 psi

Other Material Properties

Density

10 g/cm3 630 lb/ft3

Electrical Conductivity: Equal Volume

85 % IACS

Electrical Conductivity: Equal Weight (Specific)

76 % IACS

Common Calculations

Strength to Weight: Axial

7.6 points

Strength to Weight: Bending

9.3 points

Followup Questions

Further Reading

ASTM B781: Standard Guide for Silver-Cadmium Oxide Contact Material

CRC Materials Science and Engineering Handbook, 4th ed., James F. Shackelford et al. (editors), 2015