Annealed Alkali-Lime-Silica Glass (IEC 60672 Type G-110)

Annealed alkali-lime-silica glass is a grade of alkali-lime-silica glass. The graph bars on the material properties cards below compare annealed alkali-lime-silica glass to other glass and glass-ceramics (top) and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Thermal Properties

Glass Transition Temperature

530 °C 990 °F

Thermal Expansion

9.0 µm/m-K

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz

7.1

Dielectric Strength (Breakdown Potential)

28 kV/mm 1.1 V/mil

Electrical Dissipation At 1 Hz

0.022

Electrical Dissipation At 1 MHz

0.0088

Electrical Resistivity Order of Magnitude

10 10x Ω-m

Other Material Properties

Density

2.7 g/cm3 170 lb/ft3

Elastic (Young's, Tensile) Modulus

78 GPa 11 x 106 psi

Flexural Strength

34 MPa 5.0 x 103 psi

Common Calculations

Stiffness to Weight: Axial

16 points

Stiffness to Weight: Bending

53 points

Followup Questions

Further Reading

Glass: Mechanics and Technology, Eric Le Bourhis, 2007

IEC 60672-3: Ceramic and glass-insulating materials - Part 3: Specifications for individual materials