Annealed Type 2 Iron-Nickel Soft Magnetic Alloy
Annealed Type 2 magnetic alloy is Type 2 magnetic alloy in the annealed condition. The graph bars on the material properties cards below compare annealed Type 2 magnetic alloy to: otherwise unclassified iron alloys (top), all iron alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elastic (Young's, Tensile) Modulus
190 GPa 27 x 106 psi
Elongation at Break
38 %
Poisson's Ratio
0.3
Shear Modulus
72 GPa 10 x 106 psi
Tensile Strength: Ultimate (UTS)
510 MPa 74 x 103 psi
Tensile Strength: Yield (Proof)
260 MPa 37 x 103 psi
Thermal Properties
Curie Temperature
480 °C 900 °F
Latent Heat of Fusion
270 J/g
Melting Completion (Liquidus)
1420 °C 2580 °F
Melting Onset (Solidus)
1370 °C 2500 °F
Specific Heat Capacity
460 J/kg-K 0.11 BTU/lb-°F
Thermal Expansion
12 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
3.9 % IACS
Electrical Conductivity: Equal Weight (Specific)
4.2 % IACS
Otherwise Unclassified Properties
Base Metal Price
33 % relative
Density
8.4 g/cm3 520 lb/ft3
Embodied Carbon
5.9 kg CO2/kg material
Embodied Energy
81 MJ/kg 35 x 103 BTU/lb
Embodied Water
140 L/kg 17 gal/lb
Common Calculations
Resilience: Ultimate (Unit Rupture Work)
160 MJ/m3
Resilience: Unit (Modulus of Resilience)
170 kJ/m3
Stiffness to Weight: Axial
12 points
Stiffness to Weight: Bending
23 points
Strength to Weight: Axial
17 points
Strength to Weight: Bending
17 points
Thermal Shock Resistance
16 points
Alloy Composition
| Fe | 48.2 to 53 | |
| Ni | 47 to 49 | |
| Mn | 0 to 0.8 | |
| Si | 0 to 0.5 | |
| Co | 0 to 0.5 | |
| Cr | 0 to 0.3 | |
| Mo | 0 to 0.3 | |
| Cu | 0 to 0.3 | |
| C | 0 to 0.050 | |
| S | 0 to 0.030 | |
| P | 0 to 0.010 |
All values are % weight. Ranges represent what is permitted under applicable standards.
Followup Questions
Further Reading
ASTM A753: Standard Specification for Wrought Nickel-Iron Soft Magnetic Alloys (UNS K94490, K94840, N14076, N14080)
Properties and Selection: Irons, Steels and High Performance Alloys, ASM Handbook vol. 1, ASM International, 1993
CRC Materials Science and Engineering Handbook, 4th ed., James F. Shackelford et al. (editors), 2015