As Forged and Air Cooled (M10) C67500 Bronze
M10 C67500 bronze is C67500 bronze in the M10 (as forged and air cooled) condition. The graph bars on the material properties cards below compare M10 C67500 bronze to: wrought bronzes (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elastic (Young's, Tensile) Modulus
100 GPa 15 x 106 psi
Elongation at Break
33 %
Poisson's Ratio
0.3
Rockwell B Hardness
69
Shear Modulus
40 GPa 5.8 x 106 psi
Shear Strength
330 MPa 48 x 103 psi
Tensile Strength: Ultimate (UTS)
500 MPa 72 x 103 psi
Tensile Strength: Yield (Proof)
240 MPa 34 x 103 psi
Thermal Properties
Latent Heat of Fusion
170 J/g
Maximum Temperature: Mechanical
120 °C 250 °F
Melting Completion (Liquidus)
890 °C 1630 °F
Melting Onset (Solidus)
870 °C 1590 °F
Specific Heat Capacity
390 J/kg-K 0.092 BTU/lb-°F
Thermal Conductivity
110 W/m-K 61 BTU/h-ft-°F
Thermal Expansion
21 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
24 % IACS
Electrical Conductivity: Equal Weight (Specific)
27 % IACS
Otherwise Unclassified Properties
Base Metal Price
23 % relative
Density
8.0 g/cm3 500 lb/ft3
Embodied Carbon
2.8 kg CO2/kg material
Embodied Energy
47 MJ/kg 20 x 103 BTU/lb
Embodied Water
330 L/kg 39 gal/lb
Common Calculations
Resilience: Ultimate (Unit Rupture Work)
130 MJ/m3
Resilience: Unit (Modulus of Resilience)
260 kJ/m3
Stiffness to Weight: Axial
7.3 points
Stiffness to Weight: Bending
20 points
Strength to Weight: Axial
17 points
Strength to Weight: Bending
17 points
Thermal Diffusivity
34 mm2/s
Thermal Shock Resistance
16 points
Alloy Composition
| Cu | 57 to 60 | |
| Zn | 35.1 to 41.7 | |
| Fe | 0.8 to 2.0 | |
| Sn | 0.5 to 1.5 | |
| Mn | 0.050 to 0.5 | |
| Al | 0 to 0.25 | |
| Pb | 0 to 0.2 | |
| res. | 0 to 0.5 |
All values are % weight. Ranges represent what is permitted under applicable standards.
Followup Questions
Further Reading
ASTM B283: Standard Specification for Copper and Copper-Alloy Die Forgings (Hot-Pressed)
ASTM B124: Standard Specification for Copper and Copper Alloy Forging Rod, Bar, and Shapes
ASM Specialty Handbook: Copper and Copper Alloys, J. R. Davis (editor), 2001