Half-Hard (H02) C19500 Copper
H02 C19500 copper is C19500 copper in the H02 (half hard) temper. The graph bars on the material properties cards below compare H02 C19500 copper to: wrought coppers (top), all copper alloys (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Elastic (Young's, Tensile) Modulus
120 GPa 17 x 106 psi
Elongation at Break
14 %
Poisson's Ratio
0.34
Rockwell B Hardness
79
Rockwell Superficial 30T Hardness
71
Shear Modulus
44 GPa 6.3 x 106 psi
Shear Strength
310 MPa 44 x 103 psi
Tensile Strength: Ultimate (UTS)
500 MPa 73 x 103 psi
Tensile Strength: Yield (Proof)
390 MPa 57 x 103 psi
Thermal Properties
Latent Heat of Fusion
210 J/g
Maximum Temperature: Mechanical
200 °C 390 °F
Melting Completion (Liquidus)
1090 °C 2000 °F
Melting Onset (Solidus)
1090 °C 1990 °F
Specific Heat Capacity
390 J/kg-K 0.092 BTU/lb-°F
Thermal Conductivity
200 W/m-K 120 BTU/h-ft-°F
Thermal Expansion
17 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
50 % IACS
Electrical Conductivity: Equal Weight (Specific)
51 % IACS
Otherwise Unclassified Properties
Base Metal Price
31 % relative
Density
8.9 g/cm3 560 lb/ft3
Embodied Carbon
2.7 kg CO2/kg material
Embodied Energy
42 MJ/kg 18 x 103 BTU/lb
Embodied Water
310 L/kg 37 gal/lb
Common Calculations
Resilience: Ultimate (Unit Rupture Work)
66 MJ/m3
Resilience: Unit (Modulus of Resilience)
660 kJ/m3
Stiffness to Weight: Axial
7.3 points
Stiffness to Weight: Bending
18 points
Strength to Weight: Axial
16 points
Strength to Weight: Bending
16 points
Thermal Diffusivity
58 mm2/s
Thermal Shock Resistance
18 points
Alloy Composition
| Cu | 94.9 to 98.6 | |
| Fe | 1.0 to 2.0 | |
| Co | 0.3 to 1.3 | |
| Sn | 0.1 to 1.0 | |
| P | 0.010 to 0.35 | |
| Zn | 0 to 0.2 | |
| Al | 0 to 0.020 | |
| Pb | 0 to 0.020 | |
| res. | 0 to 0.2 |
All values are % weight. Ranges represent what is permitted under applicable standards.