ISO Solder Alloy 713 (IEC A38C7, Sn95.5Ag3.8Cu0.7)
Solder alloy 713 is a tin-based soldering alloy. Cited properties are appropriate for the as-fabricated (no temper or treatment) condition. A38C7 is the IEC 60672 type for this material. 713 is the ISO numeric designation. Older literature may refer to this material as S-Sn95,5Ag3,8Cu0,7, but this is now discouraged.
It has the highest tensile strength and a moderately low ductility among tin-based solder alloys.
The graph bars on the material properties cards below compare solder alloy 713 to: tin-based solder alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.
Mechanical Properties
Brinell Hardness
15
Elastic (Young's, Tensile) Modulus
51 GPa 7.4 x 106 psi
Elongation at Break
16 %
Poisson's Ratio
0.36
Shear Modulus
19 GPa 2.7 x 106 psi
Tensile Strength: Ultimate (UTS)
59 MPa 8.5 x 103 psi
Thermal Properties
Latent Heat of Fusion
62 J/g
Melting Completion (Liquidus)
220 °C 420 °F
Melting Onset (Solidus)
220 °C 420 °F
Specific Heat Capacity
220 J/kg-K 0.053 BTU/lb-°F
Thermal Conductivity
60 W/m-K 35 BTU/h-ft-°F
Thermal Expansion
22 µm/m-K
Electrical Properties
Electrical Conductivity: Equal Volume
13 % IACS
Electrical Conductivity: Equal Weight (Specific)
16 % IACS
Otherwise Unclassified Properties
Density
7.4 g/cm3 460 lb/ft3
Embodied Carbon
18 kg CO2/kg material
Embodied Energy
300 MJ/kg 130 x 103 BTU/lb
Common Calculations
Stiffness to Weight: Axial
3.8 points
Stiffness to Weight: Bending
17 points
Strength to Weight: Axial
2.2 points
Strength to Weight: Bending
4.5 points
Thermal Diffusivity
36 mm2/s
Thermal Shock Resistance
3.7 points
Alloy Composition
| Sn | 94.6 to 95.9 | |
| Ag | 3.6 to 4.0 | |
| Cu | 0.5 to 0.9 | |
| Bi | 0 to 0.1 | |
| Sb | 0 to 0.1 | |
| In | 0 to 0.1 | |
| Pb | 0 to 0.070 | |
| Au | 0 to 0.050 | |
| As | 0 to 0.030 | |
| Fe | 0 to 0.020 | |
| Ni | 0 to 0.010 | |
| Cd | 0 to 0.0020 | |
| Al | 0 to 0.0010 | |
| Zn | 0 to 0.0010 |
All values are % weight. Ranges represent what is permitted under applicable standards.
Followup Questions
Similar Alloys
Further Reading
ISO 9453: Soft solder alloys - Chemical compositions and forms