NEMA grade G-10 is a grade of NEMA laminate. The graph bars on the material properties cards below compare NEMA grade G-10 to other thermoset plastics (top) and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Compressive (Crushing) Strength

360 MPa 51 x 103 psi

Flexural Modulus

17 GPa 2.5 x 106 psi

Flexural Strength

340 MPa 50 x 103 psi

Impact Strength: Notched Izod

330 J/m 6.3 ft-lb/in

Rockwell M Hardness

110

Shear Strength

130 MPa 19 x 103 psi

Tensile Strength: Ultimate (UTS)

260 MPa 37 x 103 psi

Thermal Properties

Maximum Temperature: Mechanical

140 °C 280 °F

Thermal Expansion

9.0 µm/m-K

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 MHz

4.5

Dielectric Strength (Breakdown Potential)

18 kV/mm 0.69 V/mil

Otherwise Unclassified Properties

Density

1.8 g/cm3 110 lb/ft3

Water Absorption After 24 Hours

0.17 %

Common Calculations

Strength to Weight: Axial

40 points

Strength to Weight: Bending

50 points