Quarter-Hard 80-Silver 20-Cadmium-Oxide Alloy

Quarter-hard 80-silver 20-cadmium-oxide is 80-silver 20-cadmium-oxide in the quarter-hard temper. The graph bars on the material properties cards below compare quarter-hard 80-silver 20-cadmium-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

1.1 %

Shear Strength

220 MPa 32 x 103 psi

Tensile Strength: Ultimate (UTS)

390 MPa 56 x 103 psi

Other Material Properties

Density

9.9 g/cm3 620 lb/ft3

Electrical Conductivity: Equal Volume

70 % IACS

Electrical Conductivity: Equal Weight (Specific)

64 % IACS

Common Calculations

Strength to Weight: Axial

11 points

Strength to Weight: Bending

12 points

Followup Questions

Further Reading

ASTM B781: Standard Guide for Silver-Cadmium Oxide Contact Material