Work hardened 92-silver 8-tin-oxide is 92-silver 8-tin-oxide in the cold worked (strain hardened) condition. The graph bars on the material properties cards below compare work hardened 92-silver 8-tin-oxide to: precious metal electrical contact alloys (top), all alloys in the same category (middle), and the entire database (bottom). A full bar means this is the highest value in the relevant set. A half-full bar means it's 50% of the highest, and so on.

Mechanical Properties

Elongation at Break

34 %

Shear Strength

210 MPa 31 x 103 psi

Tensile Strength: Ultimate (UTS)

320 MPa 46 x 103 psi

Tensile Strength: Yield (Proof)

300 MPa 43 x 103 psi

Other Material Properties

Electrical Conductivity: Equal Volume

76 % IACS

Common Calculations

Resilience: Ultimate (Unit Rupture Work)

110 MJ/m3

Followup Questions

Further Reading

ASTM B844: Standard Guide for Silver-Tin Oxide Contact Material