Both cold rolled Type 2 pewter and hard drawn ASTM B596 are otherwise unclassified metals. Both are furnished in the cold worked (strain hardened) condition. There are 15 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown. Please note that the two materials have significantly dissimilar densities. This means that additional care is required when interpreting the data, because some material properties are based on units of mass, while others are based on units of area or volume.

For each property being compared, the top bar is cold rolled Type 2 pewter and the bottom bar is hard drawn ASTM B596.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 52
100
Poisson's Ratio 0.35
0.41
Shear Modulus, GPa 19
36
Tensile Strength: Ultimate (UTS), MPa 52
620

Thermal Properties

Latent Heat of Fusion, J/g 69
77
Melting Completion (Liquidus), °C 300
1060
Melting Onset (Solidus), °C 240
930
Specific Heat Capacity, J/kg-K 220
150
Thermal Expansion, µm/m-K 21
14

Otherwise Unclassified Properties

Density, g/cm3 7.3
18

Common Calculations

Stiffness to Weight: Axial, points 3.9
3.1
Stiffness to Weight: Bending, points 17
8.5
Strength to Weight: Axial, points 2.0
9.4
Strength to Weight: Bending, points 4.3
8.8
Thermal Shock Resistance, points 3.4
30

Alloy Composition


Deprecated: Automatic conversion of false to array is deprecated in /home/public/compare.php on line 460
Antimony (Sb), % 5.0 to 7.5
0
Arsenic (As), % 0 to 0.050
0
Copper (Cu), % 1.5 to 3.0
9.0 to 11
Gold (Au), % 0
89 to 91
Iron (Fe), % 0 to 0.015
0
Lead (Pb), % 0 to 0.050
0
Tin (Sn), % 90 to 93
0
Zinc (Zn), % 0 to 0.0050
0
Residuals, % 0