Elastic (Young's, Tensile) Modulus, GPa 200
190
Elongation at Break, % 34
30 to 34
Fatigue Strength, MPa 190
150 to 180
Poisson's Ratio 0.28
0.29
Shear Modulus, GPa 77
73
Tensile Strength: Ultimate (UTS), MPa 540
380 to 450
Tensile Strength: Yield (Proof), MPa 240
190 to 230

Thermal Properties

Latent Heat of Fusion, J/g 290
250
Maximum Temperature: Mechanical, °C 930
400
Melting Completion (Liquidus), °C 1420
1470
Melting Onset (Solidus), °C 1380
1420 to 1430
Specific Heat Capacity, J/kg-K 480
470
Thermal Conductivity, W/m-K 15
53
Thermal Expansion, µm/m-K 12
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 2.3
7.0
Electrical Conductivity: Equal Weight (Specific), % IACS 2.7
8.0

Otherwise Unclassified Properties

Base Metal Price, % relative 17
1.8
Density, g/cm3 7.8
7.9
Embodied Carbon, kg CO2/kg material 3.3
1.4
Embodied Energy, MJ/kg 47
18
Embodied Water, L/kg 150
46

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 150
110
Resilience: Unit (Modulus of Resilience), kJ/m3 150
94 to 150
Stiffness to Weight: Axial, points 14
13
Stiffness to Weight: Bending, points 25
24
Strength to Weight: Axial, points 19
13 to 16
Strength to Weight: Bending, points 19
15 to 17
Thermal Diffusivity, mm2/s 4.1
14
Thermal Shock Resistance, points 16
12 to 14